Bubbles appear inside or on the surface of extruded products

Problembeschreibung
Bubbles appear inside or on the surface of extruded products, voids visible in pipe or profile cross-sections
Ursachenanalyse
Raw material moisture content exceeds standard, vaporizing at high temperature Extrusion temperature too high (exceeding the upper limit of 170-230°C), thermal degradation Insufficient screw venting section, poor venting Poor die venting Regrind contains moisture
Lösung
Fully dry the raw material under 75-85°C/3-4h conditions Lower the extrusion temperature to a reasonable value of 170-230°C Ensure the screw venting section is effective Add die venting Fully dry the regrind
Wichtigste Erkenntnis
Extrusion bubbles need to be addressed from drying and venting
extrusion bubblesdryingventingtemperature