Material Drying 7 visualizações

Bubbles appear inside or on the surface of extruded products

Fenómeno do problema
Bubbles appear inside or on the surface of extruded products, voids visible in pipe or profile cross-sections
Análise das causas
Raw material moisture content exceeds standard, vaporizing at high temperature Extrusion temperature too high (exceeding the upper limit of 170-230°C), thermal degradation Insufficient screw venting section, poor venting Poor die venting Regrind contains moisture
Solução
Fully dry the raw material under 75-85°C/3-4h conditions Lower the extrusion temperature to a reasonable value of 170-230°C Ensure the screw venting section is effective Add die venting Fully dry the regrind
Conclusão principal
Extrusion bubbles need to be addressed from drying and venting