Processing Machinery 3 Aufrufe

Glass Fibre insufficient mixing

Problembeschreibung
Glass Fibre blended with filler/additives, dispersion uneven, local agglomeration
Ursachenanalyse
Screw mixing section length insufficient; kneading block number not enough; feeding method improper, additives and Glass Fibre not fully contacted
Lösung
1) Increase screw mixing section length to 3-4D; 2) increase kneading block number; 3) additives added later at side feed port to increase mixing time
Wichtigste Erkenntnis
Insufficient mixing is caused by improper screw design; increasing mixing section is key
Glass Fibreinsufficient mixingscrew mixing sectionkneading blocksside feeding