Processing Machinery 2 views

Glass Fibre insufficient mixing

Problem Phenomenon
Glass Fibre blended with filler/additives, dispersion uneven, local agglomeration
Cause Analysis
Screw mixing section length insufficient; kneading block number not enough; feeding method improper, additives and Glass Fibre not fully contacted
Solution
1) Increase screw mixing section length to 3-4D; 2) increase kneading block number; 3) additives added later at side feed port to increase mixing time
Key Takeaway
Insufficient mixing is caused by improper screw design; increasing mixing section is key
Glass Fibreinsufficient mixingscrew mixing sectionkneading blocksside feeding

Was this helpful?

0 people found this helpful