Glass Fibre insufficient mixing

Fenómeno del problema
Glass Fibre blended with filler/additives, dispersion uneven, local agglomeration
Análisis de la causa
Screw mixing section length insufficient; kneading block number not enough; feeding method improper, additives and Glass Fibre not fully contacted
Solución
1) Increase screw mixing section length to 3-4D; 2) increase kneading block number; 3) additives added later at side feed port to increase mixing time
Conclusión clave
Insufficient mixing is caused by improper screw design; increasing mixing section is key