MP extruder screw severe wear

Problembeschreibung
after 200h of MP extrusion, screw and barrel wear reaches 0.5mm
Ursachenanalyse
filler causes large screw wear; screw material hardness insufficient, not nitrided; processing temperature high causing MP adhesion to the screw, aggravating wear
Lösung
1) use a nitrided screw or bimetallic screw SK-2 alloy; 2) lower processing temperature to reduce adhesive wear; 3) treat filler with coupling agent to reduce friction; 4) regularly check wear, replace promptly when >0.3mm
Wichtigste Erkenntnis
screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are key