Surface Defect Problem in Coating of PAK Special Engineering Plastic
Problembeschreibung
Polyacrylate ketone PAK shows surface defect during coating processing at 240-300°C.
Ursachenanalyse
Improper control in the aspect of PAK high-temperature degradation).
Lösung
Increase the mold temperature.
Wichtigste Erkenntnis
PAK high-temperature processing requires precise control.