Extrusion & Post 8 views

Surface Defect Problem in Coating of PAK Special Engineering Plastic

Problem Phenomenon
Polyacrylate ketone PAK shows surface defect during coating processing at 240-300°C.
Cause Analysis
Improper control in the aspect of PAK high-temperature degradation).
Solution
Increase the mold temperature.
Key Takeaway
PAK high-temperature processing requires precise control.
PAKspecial engineering plasticsurface defectcoatinghigh temperature