PBN uneven crystallization Problem in Sheet Processing
Problembeschreibung
Polybutylene naphthalate PBN exhibits uneven crystallization in sheet processing at 270-300°C.
Ursachenanalyse
Under high-temperature processing at 270-300°C, hydrolysis causes the problem.
Lösung
Solve by optimizing the mold temperature.
Wichtigste Erkenntnis
PBN ultra-high-temperature processing requires comprehensive protection.