Material Drying
5 views
PBN uneven crystallization Problem in Sheet Processing
Problem Phenomenon
Polybutylene naphthalate PBN exhibits uneven crystallization in sheet processing at 270-300°C.
Cause Analysis
Under high-temperature processing at 270-300°C, hydrolysis causes the problem.
Solution
Solve by optimizing the mold temperature.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
Was this helpful?
0 people found this helpful
Thank you for your feedback!