2079851475616104452 cycle exceeds target by more than 20%
Ursachenanalyse
Cooling time accounts for a large proportion, plasticizing insufficient, mold opening and closing slow
Lösung
Optimize cooling water channels, increase plasticizing capacity, increase mold opening and closing speed
Wichtigste Erkenntnis
Cycle optimization is the key to increasing output and reducing cost