Injection Molding 2 views

SBS injection cycle too long affecting efficiency

Problem Phenomenon
2079851475616104452 cycle exceeds target by more than 20%
Cause Analysis
Cooling time accounts for a large proportion, plasticizing insufficient, mold opening and closing slow
Solution
Optimize cooling water channels, increase plasticizing capacity, increase mold opening and closing speed
Key Takeaway
Cycle optimization is the key to increasing output and reducing cost