SBS injection cycle too long affecting efficiency
Fenómeno do problema
2079851475616104452 cycle exceeds target by more than 20%
Análise das causas
Cooling time accounts for a large proportion, plasticizing insufficient, mold opening and closing slow
Solução
Optimize cooling water channels, increase plasticizing capacity, increase mold opening and closing speed
Conclusão principal
Cycle optimization is the key to increasing output and reducing cost