Material Drying 3 Aufrufe

PET recycled bottle flakes agglomerate after drying

Problembeschreibung
PET recycled bottle flakes agglomerate and bridge in the drying hopper and cannot feed normally.
Ursachenanalyse
Drying temperature is too high (>170°C); bottle flake surfaces soften and stick together; time is too long; low-melting-point PVC label residues are mixed in.
Lösung
Control drying temperature ≤165°C; control material level ≤70%; add a stirring device to prevent bridging; strengthen sorting to remove PVC.
Wichtigste Erkenntnis
Agglomeration of PET bottle flakes during drying is a common problem in recycling processing.