Material Drying
6 visualizaciones
PET recycled bottle flakes agglomerate after drying
Fenómeno del problema
PET recycled bottle flakes agglomerate and bridge in the drying hopper and cannot feed normally.
Análisis de la causa
Drying temperature is too high (>170°C); bottle flake surfaces soften and stick together; time is too long; low-melting-point PVC label residues are mixed in.
Solución
Control drying temperature ≤165°C; control material level ≤70%; add a stirring device to prevent bridging; strengthen sorting to remove PVC.
Conclusión clave
Agglomeration of PET bottle flakes during drying is a common problem in recycling processing.
¿Le ha resultado útil?
0 personas encontraron esto útil