Extrusion & Post 3 Aufrufe

Sharkskin on the surface of PET extruded pipes

Problembeschreibung
Regular sharkskin-like rough texture appears on the surface of PET extruded pipes, with a rough hand feel.
Ursachenanalyse
Excessive extrusion speed causes melt fracture; die head temperature is on the low side and skin viscosity is high; the die head inner wall is rough.
Lösung
Reduce extrusion speed or increase die head temperature; reduce melt viscosity (appropriately increase temperature); polish the die head inner wall.
Wichtigste Erkenntnis
PET pipe sharkskin is a typical manifestation of melt fracture.
PETpipesharkskinmelt fracturedie head temperature