Extrusion & Post 8 visualizaciones

Sharkskin on the surface of PET extruded pipes

Fenómeno del problema
Regular sharkskin-like rough texture appears on the surface of PET extruded pipes, with a rough hand feel.
Análisis de la causa
Excessive extrusion speed causes melt fracture; die head temperature is on the low side and skin viscosity is high; the die head inner wall is rough.
Solución
Reduce extrusion speed or increase die head temperature; reduce melt viscosity (appropriately increase temperature); polish the die head inner wall.
Conclusión clave
PET pipe sharkskin is a typical manifestation of melt fracture.