PETG '2079851475616104452 gate area sink mark
Problembeschreibung
Sink marks (shrinkage) appear near the gate of PETG products, affecting appearance and dimensions.
Ursachenanalyse
Insufficient holding pressure and inadequate feeding at the gate, the gate solidifies too early cutting off the feeding channel, and this area is locally overheated with large cooling shrinkage.
Lösung
Increase holding pressure and extend holding time; enlarge the gate to delay solidification; ensure the holding switchover point is accurate.
Wichtigste Erkenntnis
PETG gate sink marks are related to holding pressure transmission efficiency.