Injection Molding
8 visualizaciones
PETG '2079851475616104452 gate area sink mark
Fenómeno del problema
Sink marks (shrinkage) appear near the gate of PETG products, affecting appearance and dimensions.
Análisis de la causa
Insufficient holding pressure and inadequate feeding at the gate, the gate solidifies too early cutting off the feeding channel, and this area is locally overheated with large cooling shrinkage.
Solución
Increase holding pressure and extend holding time; enlarge the gate to delay solidification; ensure the holding switchover point is accurate.
Conclusión clave
PETG gate sink marks are related to holding pressure transmission efficiency.
¿Le ha resultado útil?
0 personas encontraron esto útil