Injection Molding
3 Aufrufe
PETG injection molded product sticking at the hot runner gate
Problembeschreibung
During demolding of PETG products, the residual sprue at the gate sticks to the hot runner nozzle opening.
Ursachenanalyse
The gate area temperature is high and melt viscosity low causing stringing, the hot runner valve pin does not close tightly, cooling insufficient and gate strength inadequate.
Lösung
Precisely control the gate area temperature; check valve pin action and sealing; strengthen cooling at the gate location.
Wichtigste Erkenntnis
PETG hot runner gate sticking requires investigation from temperature and mechanics.