Weak adhesion of PLA to paper/paperboard lamination
Problembeschreibung
The adhesion between PLA and the paper base of PLA coated paper products is insufficient.
Ursachenanalyse
The wettability of PLA to the paper base is not enough and the adhesion is weak; the surface treatment of the paper base is insufficient.
Lösung
Corona or primer treatment of the paper base; increase the PLA coating temperature to improve wettability.
Wichtigste Erkenntnis
The adhesion of PLA paper base lamination is the key to packaging.