Extrusion & Post 2 views

Weak adhesion of PLA to paper/paperboard lamination

Problem Phenomenon
The adhesion between PLA and the paper base of PLA coated paper products is insufficient.
Cause Analysis
The wettability of PLA to the paper base is not enough and the adhesion is weak; the surface treatment of the paper base is insufficient.
Solution
Corona or primer treatment of the paper base; increase the PLA coating temperature to improve wettability.
Key Takeaway
The adhesion of PLA paper base lamination is the key to packaging.
PLA coating adhesion paper base corona