Injection Molding 3 Aufrufe

Filling difficulty of thin-walled products in PLA high-speed '2079851475616104452

Problembeschreibung
Thin-wall high-speed injection of PLA is difficult to fill, resulting in under-filling.
Ursachenanalyse
The fluidity of PLA is insufficient to fill the thin wall within the extremely short filling time.
Lösung
Use high-flow PLA grades; raise the melt temperature and mold temperature.
Wichtigste Erkenntnis
PLA thin-wall high-speed '2079851475616104452 is a rheological property challenge.
PLA thin wall filling high speed