Injection Molding
4 görüntüleme
Filling difficulty of thin-walled products in PLA high-speed '2079851475616104452
Sorun Belirtisi
Thin-wall high-speed injection of PLA is difficult to fill, resulting in under-filling.
Neden Analizi
The fluidity of PLA is insufficient to fill the thin wall within the extremely short filling time.
Çözüm
Use high-flow PLA grades; raise the melt temperature and mold temperature.
Temel Çıkarım
PLA thin-wall high-speed '2079851475616104452 is a rheological property challenge.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu