Fenómeno del problema
Thin-wall high-speed injection of PLA is difficult to fill, resulting in under-filling.
Análisis de la causa
The fluidity of PLA is insufficient to fill the thin wall within the extremely short filling time.
Solución
Use high-flow PLA grades; raise the melt temperature and mold temperature.
Conclusión clave
PLA thin-wall high-speed '2079851475616104452 is a rheological property challenge.