Cracks on the Surface of acrylonitrile-styrene-acrylate copolymer Extruded Profiles

Problembeschreibung
Cracks appear on the surface of the extruded profiles, affecting the product appearance and subsequent processing quality. This problem is common in acrylonitrile-styrene-acrylate copolymer extrusion production.
Ursachenanalyse
(1)The extrusion temperature (220-260°C) is set improperly, and the melt quality is unstable (2)The screw rotation speed and the haul-off speed are improperly matched (3)Die condition or design problems (4)The cooling system is set improperly (5)Raw material quality or pretreatment problems
Lösung
(1)Optimize the extrusion temperature to a reasonable value within the 220-260°C range (2)Stabilize the screw rotation speed and the haul-off speed (3)Check the die condition, clean the accumulated material or repair the damage (4)Adjust the cooling water temperature and flow (5)Ensure the raw material is dried (70-80°C, 3-4h) and clean
Wichtigste Erkenntnis
Extrusion surface defects need to be controlled from three aspects: temperature, speed, and die condition.