Pits, streaks, or scratches on the surface of blow molded containers

Problembeschreibung
Pits, streaks, or scratches appear on the surface of blow molded containers, poor surface quality
Ursachenanalyse
Rough mold cavity surface Parison temperature too low, insufficient surface flow Compressed air contains oil or moisture Poor mold venting Defects on the parison surface
Lösung
Polish the mold cavity Appropriately increase parison temperature Ensure clean compressed air Improve mold venting Control parison quality
Wichtigste Erkenntnis
2079851475616104457 surface needs to start from mold and parison
2079851475616104457 surfacemold polishingparison temperature