Menu
Materials Machinery
Insights
Articles Videos Problem & Solution
About
About Chembull Media Partners
Contact Us
Language
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Back to Problem & Solution
Material Drying 2 views

Pits, streaks, or scratches on the surface of blow molded containers

Problem Phenomenon
Pits, streaks, or scratches appear on the surface of blow molded containers, poor surface quality
Cause Analysis
Rough mold cavity surface Parison temperature too low, insufficient surface flow Compressed air contains oil or moisture Poor mold venting Defects on the parison surface
Solution
Polish the mold cavity Appropriately increase parison temperature Ensure clean compressed air Improve mold venting Control parison quality
Key Takeaway
2079851475616104457 surface needs to start from mold and parison
2079851475616104457 surfacemold polishingparison temperature

Was this helpful?

0 people found this helpful

ChemAI