Praktische Antworten auf häufige Herausforderungen mit Kunststoffmaterialien

11636 Fragen
Q
POM short shot
A
Short shot = racing against solidification.
Molds & Tooling POM;short shot;solidification;injection speed;mold temperature
Q
POM '2079851475616104452 flash
A
Flash of low-viscosity material = pressure and gaps.
Injection Molding POM;flash;low viscosity;clamping
Q
POM sink marks and voids
A
POM feeding = gate freeze time management.
Molds & Tooling POM;sink marks;voids;gate freeze;holding pressure
Q
POM weld line weak strength
A
POM weld lines = racing against crystallization speed.
Molding Process POM;weld line;crystallization;melt temperature;gate
Q
POM surface streaks/silver streaks
A
For POM silver streaks, check degradation first, then moisture.
Material Drying POM;silver streaks;streaks;degradation;drying
Q
POM sticking to mold
A
POM mold sticking = crystallization gripping force, and increasing mold temperature is the key.
Molds & Tooling POM;mold sticking;crystallization;mold temperature;draft
Q
POM warpage
A
Warpage = a lesson in balancing crystallization shrinkage.
Molds & Tooling POM;warpage;crystallization;mold temperature;holding pressure
Q
POM product dimensions too small (post-shrinkage)
A
POM dimensions = only the dimensions after 24 hours count.
Molds & Tooling POM;post-shrinkage;dimension;crystallization;measurement aging
Q
POM trapped air burning
A
Burning = check both venting and temperature.
Molds & Tooling POM;trapped air;burning;venting;decomposition
Q
POM mold deposits (mold fouling)
A
POM mold fouling = a high-frequency maintenance item, and venting is the line of defense.
Molds & Tooling POM;mold fouling;deposition;venting;maintenance