Molds & Tooling
8 visualizaciones
Poor Surface Gloss
Fenómeno del problema
The surface gloss of the part is uneven or overall dull.
When this defect appears in parts of Process No.
1, it is usually related to specific process parameter ranges or equipment conditions.
If it persists, it will directly affect the part qualification rate and production cycle, increasing material loss and rework costs.
Timely diagnosis and elimination is a basic requirement for ensuring stable production.
Análisis de la causa
1.
Mold design factors: rough mold cavity surface, low mold temperature, low melt temperature, insufficient holding pressure, excessive release agent.
Solución
1.
Process parameter optimization and adjustment: polish the mold cavity, increase mold temperature and melt temperature, increase holding pressure, reduce the amount of release agent.
2.
Systematic troubleshooting method: troubleshoot item by item in the order of "parameters -> material -> mold -> equipment".
First adjust the parameters that are easiest to change, such as injection pressure and temperature, and observe the effect; if there is no improvement, check the drying and fluidity of the raw material; further check mold venting and gate design; finally check the mechanical condition of the equipment (check ring, screw).
Change only one variable at a time to determine the root cause.
3.
Preventive management: establish standardized process parameter cards and quality control limits for each mold/product, and regularly conduct process capability index (CPK) evaluation.
For recurring problems, use fishbone diagram or 5Why analysis to trace the root cause, and fix the countermeasures as PFMEA control points.
Conclusión clave
This problem is a typical manifestation of poor surface gloss in '2079851475616104452; the core of the solution lies in eliminating the root cause of the defect through systematic optimization of process parameters (temperature, pressure, speed) and rationality checks of mold design.
It is recommended to start with process parameter adjustment and gradually go deeper into the equipment and mold levels.