Molds & Tooling 4 visualizaciones

ABAK weld line strength

Fenómeno del problema
ABAK multi-gate products have insufficient weld line strength, under the dual influence of two-phase interface and flow convergence.
Análisis de la causa
The two phases are unevenly distributed at ABAK weld lines; the temperature of the flow front drops; compatibilizer distribution affects interfacial bonding; the weld line of the crystalline PA component is weaker; improper gate position.
Solución
①Increase melt temperature and injection speed; ②optimize gate position; ③vent the convergence area; ④optimize compatibilizer and dispersion.; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
ABAK weld lines are the weak link of the alloy; temperature, speed, and gate are all important; dispersion quality affects the interface.; After confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
ABAK;weld line;strength;gate;dispersion;venting