Molds & Tooling 8 visualizaciones

COC Demolding Damage

Fenómeno del problema
COC products crack, whiten or surface scratched during ejection, deep-cavity transparent parts have obvious ejection marks, automated demolding interruption rate high.
Análisis de la causa
COC is rigid and brittle, ejection stress concentration easily cracks; insufficient draft angle and undercut structure make demolding resistance too large; small ejector pin area concentrates pressure and damages the surface.
Solución
①Adopt as large draft angle as possible (refer to polystyrene standard); ②minimize undercuts; ③configure sufficient number of large-area ejector pins or stripper plate demolding; ④optimize ejection speed curve for slow start.
Conclusión clave
COC demolding design standard aligns with PS; large draft angle and large-area ejection are the two iron rules; ejection damage prevention of brittle materials beats all post-remediation.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
COC; demolding; ejector whitening; draft angle; ejector pin; brittleness