Extrusion & Post 3 visualizaciones

HDPE film gel (fisheye)

Fenómeno del problema
HDPE blown film has gel spots and fisheyes, and the film surface of high-strength shopping bags is defective.
Análisis de la causa
Unplasticized particles, degraded crosslinked material or impurities; HDPE has high molecular weight and is difficult to plasticize, and gel is more obvious when the screen is insufficient.
Solución
①Increase plasticization temperature and mixing (barrier screw + mixing section); ②densify the screen; ③clean the dead corners of the head; ④control regrind quality.
Conclusión clave
Plasticization of high molecular weight material is the foundation of gel prevention and control.
HDPE; blown film; gel; fisheye; plasticization