Extrusion & Post 3 visualizaciones

HDPE film poor opening

Fenómeno del problema
Two layers of the film stick together after winding, making bag opening difficult.
Análisis de la causa
Insufficient slip/anti-blocking agent in HDPE film or slow migration; high winding tension and high film temperature aggravate blocking.
Solución
①Add/adjust anti-blocking agent and slip agent; ②reduce winding tension; ③fully cool the bubble before winding; ④control storage temperature.
Conclusión clave
Opening is controlled by three controls: additives + tension + temperature.