Processing Machinery 11 visualizaciones

HDPE equipment screw

Fenómeno del problema
HDPE plasticization is uneven, unmelted particles appear in the product, and back pressure adjustment has limited effect
Análisis de la causa
HDPE is suitable for general-purpose screws with a compression ratio of 2.0-3.0; too low a compression ratio causes insufficient plasticization, and too high causes large shear heat; back pressure only needs to ensure melt uniformity, and too high is useless
Solución
①Screw compression ratio 2.0-3.0; ②back pressure at the low limit to ensure uniformity; ③for poor plasticization check screw wear and temperature; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
HDPE screw selection is lenient but has boundaries; a 2.0-3.0 compression ratio plus low back pressure is the standard configuration; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
HDPE; screw; compression ratio; back pressure; plasticization