Extrusion & Post 4 visualizaciones

Sharkskin on LCP Extruded Profile Surface

Fenómeno del problema
【Problem Phenomenon】Periodic rough sharkskin patterns appear on the surface of LCP extruded rods or sheets
Análisis de la causa
Alternating slip-stick of the melt at the die wall causes melt fracture, and sharkskin appears when the shear rate reaches a critical value; high-temperature low-viscosity LCP also has critical shear problems in high-output extrusion
Solución
Reduce the extrusion line speed or raise the die temperature to reduce shear stress; polish the die flow channel to reduce resistance; if necessary, add processing aids to promote wall slip; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Sharkskin is a signal of shear exceeding the critical value; lowering temperature and raising speed is not as good as matching speed increase with temperature decrease; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
extrusion sharkskin melt fracture die