Molding Process 8 visualizaciones

LDPE Film Longitudinal Splitting (Splitty)

Fenómeno del problema
The film tears very easily along the longitudinal direction, and TD strength is low.
Análisis de la causa
Too small blow-up ratio and too large draw ratio cause excessive longitudinal molecular orientation; improper frost line height also aggravates it.
Solución
①Increase the blow-up ratio; ②reduce the draw ratio; ③optimize frost line height; ④select grades with wider molecular weight distribution.
Conclusión clave
Longitudinal splitting = orientation imbalance; adjust the blow-up ratio.