Extrusion & Post
2 visualizaciones
LLDPE blown film gel particles
Fenómeno del problema
Gel particles and fish eyes scattered on the film surface; high-end packaging film customers reject.
Análisis de la causa
LLDPE plasticization requires stronger mixing shear; unmelted particles, cross-linked gel, and impurities enter the film with the melt forming visible defects.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Solución
①Use a barrier screw with a mixing section; ②increase screen precision and replace regularly; ③clean die head dead spots; ④strengthen raw material inspection.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Conclusión clave
LLDPE has higher requirements on screw plasticization capability than LDPE; equipment upgrading and enhanced filtration are the core of gel particle control.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.