Injection Molding 3 visualizaciones

PA6 '2079851475616104452 Black Specks

Fenómeno del problema
Black specks and black streaks, obvious on light-color parts.
Análisis de la causa
Dead corner carbonization (PA carbonization is obvious at high temperature), raw material contamination; high-temperature nylon dead corner accumulated material easily carbonizes; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solución
①Thoroughly clean the machine to remove accumulated material in the dead corners of the barrel and hot runner;②avoid long-time high-temperature idling heat preservation of the barrel;③check the cleanliness of raw material and regrind to eliminate pollution sources;④use purging material to thoroughly replace during material change;⑤establish a regular machine cleaning and maintenance system to prevent dead corner material accumulation.
Conclusión clave
PA6 black specks = 'carbonization': dead corners are the root; nylon processing temperature is high, dead corner accumulated material carbonizes quickly, and machine cleaning and maintenance must be normalized; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
PA6; black specks; carbonization; dead corners