Extrusion & Post 3 visualizaciones

PA66 product delamination

Fenómeno del problema
Layered peeling, more frequent near the gate.
Análisis de la causa
Mixed material contamination, excessive release agent; layers cannot fuse; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; during troubleshooting, confirm item by item around key factors such as delamination and contamination to avoid misjudgment.
Solución
①Troubleshoot material mixing and contamination, standardize storage management of virgin material and regrind; ②thoroughly clean the machine, removing accumulated material in dead corners of the barrel and hot runner; ③control release agent usage to avoid forming an isolation layer on the surface; ④strengthen raw '2079851475616104451 and verify moisture content compliance by moisture determination; ⑤check regrind compatibility.
Conclusión clave
PA66 delamination='contamination': mixing in incompatible material is the primary cause; nylon and polyolefin are incompatible, mixing materials is a major taboo; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA66; delamination; contamination; release agent