PARA Dents and Sink Marks

Fenómeno del problema
Dents in thick-wall areas of PARA products; multiple factors of insufficient filling, improper gate, uneven wall thickness and insufficient holding.
Análisis de la causa
Insufficient filling feed or inadequate feeding amount; improper or asymmetric gate position; insufficient or too-small sub-runners and gates; uneven product wall thickness; insufficient holding pressure and time.
Solución
①Increase feeding or open the feed port gate plate; ②Adjust gate position and symmetry; ③Add sub-runners and enlarge gate size; ④Increase injection pressure and holding.
Conclusión clave
Systematic troubleshooting of PARA dents covers feeding, gate, runner, wall thickness and holding; uniform wall thickness is the design foundation; holding optimization is the process means.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PARA; dent; filling; gate; wall thickness; holding