PARA Metallization

Fenómeno del problema
PARA metallization coating bonding is poor; surface state and pretreatment.
Análisis de la causa
PARA metallization surface energy; glass fiber influence; roughening and activation; coating stress.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
Solución
①Surface roughening and activation treatment; ②Glass fiber surface management; ③Coating process matching; ④Bond strength testing.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Surface engineering of PARA metallization is key; roughening and activation are standard procedures; testing ensures quality.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PARA; metallization; coating; roughening; activation; bond strength