Injection Molding
3 visualizaciones
PBAT '2079851475616104452 warpage
Fenómeno del problema
PBAT injection molded products warp and deform, with uneven crystallization and internal stress acting together.
Análisis de la causa
PBAT crystallization rate is slow; uneven cooling causes shrinkage differences; improper holding pressure causes internal stress; uneven wall thickness; high demolding temperature.; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
①Uniform control of mold temperature; ②optimize holding pressure curve; ③uniform wall thickness design; ④sufficient cooling time; ⑤annealing treatment.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Cooling uniformity is the core of PBAT warpage; holding pressure and structure are equally important; annealing is a post-treatment option.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence