Injection Molding 3 visualizaciones

PC Injection Machine Screw Wear Acceleration

Fenómeno del problema
After processing glass fiber reinforced PC, the screw and check ring wear quickly, and metering fluctuates.
Análisis de la causa
Glass fiber strongly wears metal, and ordinary nitrided screws have a short service life; after wear, plasticizing and metering become unstable, and product quality fluctuates.
Solución
①Use bimetallic/hardened screws and barrels for GF-PC; ②Regularly check the check ring clearance; ③Monitor the trend of plasticizing time changes.
Conclusión clave
Glass fiber material must be equipped with a wear-resistant plasticizing system.
PC; glass fiber; screw wear; metering; bimetallic