Molds & Tooling 7 visualizaciones

PC/ABS ejector whitening

Fenómeno del problema
Whitening at ejection positions.
Análisis de la causa
Ejection force concentrated, stress whitening; insufficient cooling, large clinging force.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solución
①Increase ejection area; ②extend cooling; ③balance ejection; ④ensure demolding draft.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Ejector whitening is a signal of local stress overload.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
PC/ABS;ejector whitening;ejection;stress;cooling;draft