PC annealing treatment specification
Fenómeno del problema
【Problem Phenomenon】PC products have large internal stress, no annealing treatment done
Análisis de la causa
PC annealing 120-130℃×1-2h eliminates internal stress; high-stress parts, insert parts, electroplated parts must be annealed; slow cooling after annealing;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solución
High-stress parts annealed at 120-130℃×1-2h; slow cooling; stress verified after annealing;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PC annealing 120-130℃ eliminates stress, high-stress parts must do it;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!