PC Black Specks Thermal Decomposition
Fenómeno del problema
[Problem Phenomenon] Black specks on light-colored PC products, recurring after cleaning
Análisis de la causa
Carbonization in barrel dead corners, hot runner material buildup, regrind contamination, degradation above 320°C; black specks are stubborn; when troubleshooting on site, verify each item according to this mechanism one by one, and avoid blindly adjusting the machine based on experience alone
Solución
Clean the barrel and hot runner and check dead corners; clean regrind; melt temperature ≤320°C; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Conclusión clave
For PC black specks, check dead corners and regrind; degradation above 320°C is the root; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!