Molds & Tooling
7 visualizaciones
PLA product warpage
Fenómeno del problema
Products warp and deform after demolding.
Análisis de la causa
Uneven cooling and uneven crystallization act together; PLA crystallization behavior is temperature sensitive.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
① Balance the cooling system; ② uniform mold temperature; ③ optimize holding pressure; ④ improve crystallization uniformity.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PLA warpage must be managed from both cooling and crystallization ends.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!