Material Analysis 15 visualizaciones

PMMA First Article Optical Verification

Fenómeno del problema
Optical defects found after mass production of transparent parts; the first article only underwent dimensional inspection
Análisis de la causa
Dimensional inspection cannot find defects such as haze, stress patterns, and weld lines on PMMA optical parts; the first article must include light transmittance and stress inspection to intercept batch risks
Solución
①First article undergoes four verifications: appearance, dimensions, light transmittance, and stress; ②check stress distribution with a polarizer; ③mass production after parameter locking; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability
Conclusión clave
First articles of PMMA optical parts must be optically examined; four verifications plus polarized stress inspection are the institutional bottom line; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PMMA;first article verification;light transmittance;polarized light;optics