PP Hot Runner Temperature

Fenómeno del problema
[Problem Phenomenon] PP hot runner gate defects; improper temperature control
Análisis de la causa
Hot runner temperature matched with the barrel at 220-260°C; local overheating degrades and low temperature causes cold material; PP's good fluidity makes gates prone to drooling; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Solución
Hot runner 220-260°C zoned closed-loop; gate drool prevention; regularly check thermocouples; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PP hot runner 220-260°C; drool prevention is the focus; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
hot runner temperature control drooling gate